parkerizing metal prep...
I was going to "blast" parts but then I ran across old thread that mentioned using 1 part muriatic acid and 4 parts water to strip off the old finish and etch the metal.
Any opinions on this technique?
Will it also remove small amounts of rust?
Do I need to do any additional prep after this before dropping the parts in the tank (washing, additional degreasing, etc.)?
Any opinions on this technique?
Will it also remove small amounts of rust?
Do I need to do any additional prep after this before dropping the parts in the tank (washing, additional degreasing, etc.)?
0
-
I use full strength muriatic acid in my shop to clean steel. It strips rust really well, but I haven't used it diluted so I wouldn't know for sure on that. It will also etch the surface. I don't know if it's the correct finish for parkerizing, but it looks close to me. 0 -
We just bead blast any parts and wash them in solvent before dunking them. 0